Previous issues
Volume 12 Issue 4
-
Introduction to Nondestructive Testing
- 정용무
- Journal of KWJS. 1994;12(4):1-10.
-
Defect Evaluation of Steel Welds by ultrasonic Testing
- 이의종
- Journal of KWJS. 1994;12(4):11-20.
-
Update Application of Ultrasonic Flaw Detector
- 조정상
- Journal of KWJS. 1994;12(4):21-34.
-
Method of Radiographic Testing and Industrial Application
- 이용
- Journal of KWJS. 1994;12(4):35-40.
-
A Study on the Welding Process of High Strength Steel Pipe in GTAW-SMAW and SAW
- 이철구, 조선근
- Journal of KWJS. 1994;12(4):41-49.
-
Brazing Technology and Trend in Japan ( 1 ) - Aluminum Brazing -
- 정재필, 강춘식, 박영조, 황선효
- Journal of KWJS. 1994;12(4):50-62.
-
A Study on the Stress Corrosion Cracking Evaluation for Weld Joint of Steel by Using Miniaturized Small Specimen
- 유효선, 임재규, 정세희
- Journal of KWJS. 1994;12(4):63-75.
-
Effect of Ca on Droplet Transfer Phenomena in GMA Welding
- 안영호, 방국수, 이종봉, 장래웅
- Journal of KWJS. 1994;12(4):76-84.
-
Hardening Characteristics of Aluminum Alloy Surface by PTA Overlaying with Metal Powders ( I ) - Optimum condition for formation and microstructure of thicker surface alloyed layer -
- 이규천, 中田一博, 강원석, 이영호, 松田福久
- Journal of KWJS. 1994;12(4):85-101.
-
Hardening Characteristics of Aluminum Alloy Surface by PTA Overlaying with Metal Powders ( II ) - Hardening characteristics and wear resistance of thicker surface alloyed layer -
- 이규천, 中田一博, 강원석, 이영호, 松田福久
- Journal of KWJS. 1994;12(4):102-109.
-
A Study on Bondability of Electronic Materials by Different Heat Sources
- 신영의, 양협, 김경섭
- Journal of KWJS. 1994;12(4):110-116.
-
A Study of Resistance of Fatigue Crack in Aluminum Alloy Plate Bonded with FRP
- 윤한기, 오세욱, 박원조, 허정원
- Journal of KWJS. 1994;12(4):117-126.
-
A Study on the Resistance Spot Welding of Aluminum Alloy ( I )
- 김상필, 홍태민, 장희석
- Journal of KWJS. 1994;12(4):127-140.
-
The X-Ray Study on Macrostress and Microstress for Two-Phase Stainless Steel
- 오세욱, 김득진, 廣瀨幸雄
- Journal of KWJS. 1994;12(4):141-150.
-
A Study on Fatigue Strength Characteristics of Weld Joint using Metal Type Flux Cored Wire
- 강성원, 신동진, 김환식
- Journal of KWJS. 1994;12(4):151-161.